Electrical Machine Design MCQs with Explanations and Theory
This chapter covers the machine-design questions that recruitment tests repeat most: conducting materials and resistance; magnetic materials, silicon and grain-oriented steel, hysteresis and eddy loss; magnetic circuits and magnetic pull; solid, liquid and gaseous insulation, dielectric strength, dielectric loss and thermal classes; transformer construction, the emf and output equations, tests, efficiency, regulation, oil, cooling and protection; DC machine windings, the output equation, poles, commutation, shafts and bearings; induction motor air gap, slots, skew, rotor design, power factor and losses; AC windings, pitch factor and harmonics, alternator rotors, damper windings; and duty cycles, heating curves, rms loading and hydrogen cooling. Every numerical uses one or two steps, and typical design values are given with their conditions.
What you will learn
- Compare copper, aluminium and special conducting alloys and use R = ρl/A.
- Classify magnetic materials by relative permeability and explain why silicon, grain-oriented steel and laminations reduce core loss.
- Use B = Φ/A, F = NI = Φℜ and F = B²A/(2μ₀) for simple magnetic-circuit and pull numericals.
- Choose suitable solid, liquid and gaseous insulation, and relate dielectric strength, dielectric loss, moisture and thermal class.
- Apply E = 4.44fNΦm, the maximum-efficiency condition and the regulation formula to transformer numericals, and state what the OC and SC tests measure.
- Use E = PΦZN/(60A), τ = πD/P, f = PN/120 and the output equation (P ∝ D²L) for DC machine design questions.
- Explain how air gap, slot type, slot combination and skew affect induction-motor power factor, noise, cogging and starting.
- Find pitch factor, electrical angle, slip, rotor frequency, heating-curve values and rms-equivalent loads, and select a duty class and enclosure.
Topics in this chapter
| # | Topic | Access |
|---|---|---|
| 18.1 | Conducting Materials Resistance and resistivity, copper versus aluminium, annealed and hard-drawn copper, ACSR, resistance alloys, contact metals and fuse wires. | Free (below) |
| 18.2 | Magnetic Materials and Their Classes Diamagnetic, paramagnetic, ferromagnetic and ferrimagnetic materials, permalloy, the Curie point, soft and hard magnetic materials and magnetostriction. | Premium |
| 18.3 | Electrical Steel and Core Loss Silicon steel, cold-rolled grain-oriented steel, laminations, hysteresis and eddy-current loss and how they depend on frequency, flux density and thickness. | Premium |
| 18.4 | Magnetic Circuits and Magnetic Pull Flux density, mmf, reluctance, the air-gap ampere-turns, the force on a pole face, and why iron needs much less magnetising current than air or wood. | Premium |
| 18.5 | Insulating Materials Requirements of insulation; ceramics, glass and mica; polymers such as PVC, PTFE, neoprene and rubber; varnishes and waxes; liquid and gaseous insulants including SF₆. | Premium |
| 18.6 | Dielectric Properties and Thermal Classes Dielectric strength and breakdown, dielectric loss and tan δ, the effect of moisture, electrode geometry in tests, and the insulation thermal classes Y to C. | Premium |
| 18.7 | Transformer Construction and Design Core-type and shell-type construction, stepped cores, stacking and window space factors, the emf and output equations, windings, taps, impulse strength and hum. | Premium |
| 18.8 | Transformer Losses, Tests, Efficiency and Regulation No-load current, kVA rating, open- and short-circuit tests, maximum and all-day efficiency, regulation at lagging and leading power factor, and the effect of voltage and frequency on losses. | Premium |
| 18.9 | Transformer Oil, Cooling, Protection and Welding Transformers Heat transfer, oil functions and properties, contaminants, ambient temperature and overload, Buchholz relay, breather, scaling of similar machines and welding transformers. | Premium |
| 18.10 | DC Machine Design and Windings The emf and torque equations, lap and wave windings, pitches, equalisers, the output equation and specific loadings, pole pitch, choice of poles, current density, scaling and commutation. | Premium |
| 18.11 | Shafts, Bearings, Frames and DC Machine Faults Shaft material and critical speed, ball, roller and journal bearings, lubrication, slot wedges, the yoke, and common DC motor faults. | Premium |
| 18.12 | Induction Motor Design: Air Gap, Slots and Skew Synchronous speed and slip, the output equation and typical loadings, L/τ ratios, the air-gap trade-off, slot types, slot combinations, cogging, cusps and skewing. | Premium |
| 18.13 | Induction Motor Rotors, Power Factor and Losses Cage and wound rotors, deep-bar and double-cage rotors, rotor power division, the torque–slip relation, power factor and efficiency trends, leakage reactance, losses, crawling and noise. | Premium |
| 18.14 | AC Windings and Synchronous Machines Electrical angle, phase spread, pitch and distribution factors, chording to remove harmonics, parallel paths, salient and cylindrical rotors, SCR, air gap, damper windings, hunting and excitation. | Premium |
| 18.15 | Duty Cycles, Heating, Enclosures and Cooling Continuous, short-time and intermittent duties, overload capability, the heating and cooling curves, thermal time constant, rms-equivalent load, enclosures and hydrogen cooling. | Premium |
Free topic 18.1: Conducting Materials
Resistance and resistivity, copper versus aluminium, annealed and hard-drawn copper, ACSR, resistance alloys, contact metals and fuse wires.
A material with very low resistivity that carries current with little loss. In machines, conductors form the windings, bars, rings, contacts and leads. The choice affects copper loss, temperature rise, weight, size and cost.
| Resistivity | Ω·m (or Ω·mm²/m) | |
| Length | m | |
| Cross-sectional area | m² (or mm²) | |
| Temperature coefficient of resistance | 1/K |
Resistance of a copper conductor
- ρ = 0.01724 Ω·mm²/m, l = 100 m, A = 2 mm².
- R = 0.01724 × 100 / 2.
Copper and aluminium (approximate)
| Property | Copper | Aluminium ÷ copper |
|---|---|---|
| Resistivity at 20 °C | 0.01724 Ω·mm²/m | ≈ 1.62 (so 1.62 × the area for equal resistance) |
| Density | 8890 kg/m³ | ≈ 0.30 (much lighter) |
| Thermal conductivity | High | ≈ 0.57 |
Where each conductor is used
- Annealed (soft) copper: ductile — machine windings, flexible wires, cable conductors.
- Hard-drawn copper: work-hardened, higher tensile strength — overhead lines and contact wires.
- ACSR: aluminium strands carry most of the current; the steel core gives tensile strength.
- Silver: contacts (best conductivity). Tungsten: very high melting point (lamp filaments, arcing contacts).
- Manganin and constantan: very low temperature coefficient — precision and standard resistors. Nichrome: heating elements.
Mechanical terms: ductility = can be drawn into wires; malleability = can be beaten or rolled into sheets; elasticity = regains shape after load; toughness = absorbs energy before fracture.
Fuses: heat produced is I²R, so it grows with the square of current. The fusing current depends on the material, diameter, length and how well heat is carried away. For round wires the empirical Preece law gives fusing current roughly ∝ d^1.5. A 10 SWG wire is about 3.25 mm in diameter.
Solved Electrical Machine Design MCQs
10 of the 398 questions in this chapter. Choose an option, then read the explanation.
Show answer
Answer: A. 1.72 × 10⁻⁸ Ω·m Copper conducts about 1.6 times better than aluminium, so its resistivity is about 2.83/1.64 ≈ 1.72 × 10⁻⁸ Ω·m (0.01724 Ω·mm²/m). Why not the others: 4.6 × 10⁻⁸ multiplies by the ratio instead of dividing; 10⁻⁶ and 10⁻⁷ are wrong by factors of 100 and 10 — values like these belong to alloys, not copper.
Show answer
Answer: B. Hard-drawn copper Cold drawing work-hardens copper, raising its tensile strength, so hard-drawn copper is used for overhead lines and contact wires. Why not the others: annealing (with or without tinning) softens copper for windings and flexible cords; cast copper is weak and porous.
Show answer
Answer: B. Machine windings, flexible wires and cables Annealing makes copper soft and ductile, so it bends and winds easily without cracking — ideal for windings, flexible wires and cable conductors. Why not the others: overhead lines need hard-drawn copper; cores need magnetic steel; copper is non-magnetic and cannot be a permanent magnet.
Show answer
Answer: B. The aluminium strands Aluminium has far lower resistivity than steel, so it carries most of the current; the galvanised steel core mainly provides tensile strength (it may carry a small share). Why not the others: steel is a poor conductor; current divides by conductance, not equally; the thin oxide layer is an insulator.
Show answer
Answer: B. Ductility Ductility is the ability to deform plastically under tension, so a metal can be drawn into wire. Why not the others: malleability is the ability to be hammered or rolled into sheets; elasticity is returning to shape after load; toughness is absorbing energy before fracture.
Show answer
Answer: B. Contact material Silver has the highest conductivity of all metals and its oxide conducts, so it gives low, stable contact resistance in relays, switches and breakers. Why not the others: heating elements need high resistivity (nichrome); laminations need magnetic steel; slot liners are insulators.
Show answer
Answer: D. I² Formula: P = I²R. Doubling the current gives four times the heating, which is why a fuse melts quickly on a fault. (The final temperature also depends on how fast heat escapes.) Why not the others: heating is not linear in current, and it rises, not falls, with current.
Show answer
Answer: B. Its diameter, material and heat dissipation A fuse melts when the I²R heat exceeds the heat it can lose. So its material (resistivity, melting point), diameter, length and surroundings (cooling) set the fusing current. Preece’s empirical law gives I ∝ d^1.5 for round wires. Why not the others: voltage, frequency and load type do not set the melting current of the element.
Show answer
Answer: B. 3.25 mm On the British Standard Wire Gauge, 10 SWG is 0.128 inch ≈ 3.25 mm. Larger gauge numbers mean thinner wires. Why not the others: 1.0 mm is about 19 SWG; 0.32 mm is about 30 SWG; the gauge number is not the diameter in millimetres.
Show answer
Answer: C. To reduce eddy-current and skin-effect losses In a large solid conductor the leakage flux induces circulating (eddy) currents and crowds the current to one side (skin and proximity effects), raising AC loss. Insulated, transposed strands break up these paths. Why not the others: stranding does not reduce DC resistance (insulation even takes space); copper stays non-magnetic; the aim is lower AC loss, not a higher current density.
Try the free preview in the app, then unlock the full chapter with OhmPK Premium.